Problem Phenomenon
• The phenomena of layer pattern issues can be divided into two types: one is regular layer patterns, which are relatively rare; the other is irregular layer patterns, which are more common.
• Regular layer pattern: Z-axis mechanical issue
• Irregular layer striations: slicing issues, release film loosening
Solution
Regular Layered Pattern
• Problem phenomenon: The lines are uniform, appear periodically, have a fixed spacing, and are usually related to the pitch of Z-axis movement.
Cause analysis Z-axis mechanical system issue
1. The screw, guide rail, or motor itself has insufficient precision or is worn out.
2. Z-axis movement is not smooth: the lead screw is bent, there are foreign objects on the guide rail, or lubrication is insufficient, causing the platform to become laggy or jump at specific positions.
3. Assembly issues: such as the Z-axis motor being misaligned with the lead screw, or interference between the brass nut and the lead screw.
Improvement Suggestions
1. Mechanical inspection: Check the lead screw for visible bending or wear. Manually move the Z-axis slowly throughout its entire travel to feel if there are any obvious laggy points.
2. Cleaning and Lubrication: Regularly clean the lead screw and guide rail, and use special lubricating oil or grease for maintenance to ensure smooth operation.
3. Recalibration: Loosen the screws securing the Z-axis motor or brass nut, let the Z-axis run through a few full strokes to eliminate assembly stress, then retighten at the middle position, which helps resolve interference caused by improper installation.
4. Hardware Upgrade: For old or low-precision devices, regular layer lines may be an inherent defect. Currently, some high-end models have managed to control the repeat positioning error within the micron level by adopting high-precision C5-grade lead screws, strengthening guide rails, and finely adjusting the Z-axis module, thereby significantly reducing or even eliminating regular layer lines at the root.
Irregular layer pattern
• Problem Phenomenon: The texture is random with no fixed intervals, and local misalignment, faults, or overall roughness may occur
Cause Analysis
1. Insufficient model support: The support density or strength is inadequate, causing the model to slightly shake during the printing process and resulting in layer misalignment.
2. Improper slicing parameters: For example, settings such as exposure time and lift speed are unreasonable.
3. Release film slack: Affects the release effect at the bottom of the resin tank, leading to abnormal peeling force.
4. Printing environment changes: such as temperature fluctuations affecting resin viscosity.
Improvement Suggestions
1. First, check the support: This is the most common cause. Increase the support density in critical areas (especially under large overhanging surfaces) and appropriately thicken the support contact points to ensure the model is absolutely stable during the printing process.
2. Optimize slicing parameters:
• Exposure Time: Insufficient exposure can lead to incomplete curing of a single layer, resulting in poor adhesion to the previous layer and delamination. Calibration should be performed based on the resin model and Computer Performance.
• Lifting speed: If the speed is too fast and the peeling force is too large, it may pull the incompletely cured model off the support or cause layer misalignment. For large models, the lifting speed should be appropriately reduced.
3. Check the release film: Regularly check whether the release film in the magazine is loose. If it is loose, adjust or replace it according to the instruction manual to ensure its tension is appropriate.
4. Equipment Maintenance: Before printing, check whether there are any cured residues from the previous print in the material tank and on the screen, as any tiny residue may affect the flatness of the next layer.